Electrical Properties Metric English Comments
Surface Resistance 4.00e+17 ohm
4.00e+17 ohm
ASTM D257
Solvay Specialty Polymers Torlon® 4275 Polyamide-imide (PAI)  (Unverified Data**)
Torlon 4275 is a wear-resistant grade of polyamide-imide (PAI). This grade offers an excellent balance of mechanical properties and wear resistance. It offers high tensile strength and modulus with ..
Surface Resistance 4.00e+17 ohm
4.00e+17 ohm
ASTM D257
Solvay Specialty Polymers Torlon® 4275 Polyamide-imide (PAI)
Torlon® 4275 is a wear-resistant grade of polyamide-imide (PAI). This grade offers an excellent balance of mechanical properties and wear resistance. It offers high tensile strength and modulus w..
Surface Resistance >= 4.00e+17 ohm
>= 4.00e+17 ohm
ASTM D257
SABIC Innovative Plastics NORYL NH8006 PPE+HIPS
Noryl* NH8006 resin is a 30% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve a UL94 V0 flame rating (color specific) while offering an exceptio..
Surface Resistance 4.00e+17 - 5.00e+17 ohm
4.00e+17 - 5.00e+17 ohm
ROA; IEC 60093
SABIC Innovative Plastics NORYL NH8006 PPE+HIPS
Noryl* NH8006 resin is a 30% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve a UL94 V0 flame rating (color specific) while offering an exceptio..
Surface Resistance >= 4.00e+17 ohm
>= 4.00e+17 ohm
ASTM D257
SABIC Innovative Plastics NORYL NH8006 PPE+HIPS (Asia Pacific)
Noryl* NH8006 resin is a 30% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve a UL94 V0 flame rating (color specific) while offering an exceptio..
Surface Resistance 4.00e+17 - 5.00e+17 ohm
4.00e+17 - 5.00e+17 ohm
ROA; IEC 60093
SABIC Innovative Plastics NORYL NH8006 PPE+HIPS (Asia Pacific)
Noryl* NH8006 resin is a 30% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve a UL94 V0 flame rating (color specific) while offering an exceptio..
Surface Resistance >= 4.00e+17 ohm
>= 4.00e+17 ohm
ASTM D257
SABIC Innovative Plastics NORYL NH8006 PPE+HIPS (Europe-Africa-Middle East)
Noryl* NH8006 resin is a 30% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve a UL94 V0 flame rating (color specific) while offering an exceptio..
Surface Resistance 4.00e+17 - 5.00e+17 ohm
4.00e+17 - 5.00e+17 ohm
ROA; IEC 60093
SABIC Innovative Plastics NORYL NH8006 PPE+HIPS (Europe-Africa-Middle East)
Noryl* NH8006 resin is a 30% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve a UL94 V0 flame rating (color specific) while offering an exceptio..
Surface Resistance 4.00e+17 ohm
4.00e+17 ohm
IEC 60093
Polyplastics Duranex® 7407 Polybutylene Terephthalate (PBT), Super low warpage, GF filled