Electrical Properties Metric English Comments
Surface Resistance 1.00e+10 - 2.40e+16 ohm
1.00e+10 - 2.40e+16 ohm
Average value: 5.49e+15 ohm Grade Count:13
Overview of materials for Polycarbonate/ASA Alloy, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ASA Alloy, Unreinforced". Each property range of values reported is minimum and maximum va..