Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 1.50e+10 - 1.00e+12 ohm | 1.50e+10 - 1.00e+12 ohm | Average value: 3.04e+11 ohm Grade Count:4 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Ether Grade". Each property range of values reported is minimum a.. |
|||
Surface Resistance | 1.50e+10 ohm | 1.50e+10 ohm | |
Industrial Laminates/Norplex MC511A Glass Fabric Description: MC511A is a high strength, glass epoxy laminate that is specially formulated to meet power generation producer's exacting standards where higher strength at elevated temperatures ar.. |