Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Breakdown | 9500 V @Thickness 0.0500 mm |
9500 V @Thickness 0.00197 in |
1/4 inch electrode; ASTM D149 |
Victrex® APTIV® 1000-050 Polyetheretherketone (PEEK) Polymer Film, Semi-Crystalline APTIV PEEK 1000 series films are the unfilled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance applications.APTI.. |
|||
Dielectric Breakdown | 9500 V @Thickness 0.0500 mm |
9500 V @Thickness 0.00197 in |
ASTM D149 |
Victrex® APTIV® 2000-050 Polyetheretherketone (PEEK) Polymer Film, Amorphous APTIV PEEK 2000 series films are the unfilled amorphous films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance applications.APTIV PEEK .. |