Polymer Property : Dielectric Breakdown = 60000 V Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Breakdown 60000 V

@Thickness 1.57 mm
60000 V

@Thickness 0.0620 in
Cond D-48/50; ASTM D229 S/S
Industrial Laminates/Norplex NP130HF Glass Fabric
Description: High flexural, impact and tensile strength glass fabric epoxy laminate, especially in the machine direction. Engineered to provide better physical properties than NEMA FR-4. More dimens..
Dielectric Breakdown 60000 V

@Thickness 1.57 mm
60000 V

@Thickness 0.0620 in
Cond A; ASTM D229 S/S
Industrial Laminates/Norplex NP511 Glass Fabric
Description: Woven glass fabric with high temperature epoxy resin. Excellent mechanical strength and electrical properties at elevated temperatures. Continuous operating temperature is 165°C. Mat..
Dielectric Breakdown 60000 V

@Thickness 1.57 mm
60000 V

@Thickness 0.0620 in
Cond A; ASTM D229 S/S
Industrial Laminates/Norplex NP600 Paper Base Laminate
Description: A paper-base laminate with low phenolic resin content for hard, flat surfaces. This material is most commonly used for drill entry material in the PCB industry. Thickness Tested: 0.062"..
Dielectric Breakdown 60000 V

@Thickness 1.57 mm
60000 V

@Thickness 0.0620 in
Cond A; ASTM D229 S/S
Industrial Laminates/Norplex NP602 Paper Base Laminate
Description: A paper-base laminate with low phenolic resin content for hard, flat surfaces. It is typically hot punched for numerous low voltage, less than 250 volts, electrical applications.Thickne..
Dielectric Breakdown 60000 V

@Thickness 1.57 mm
60000 V

@Thickness 0.0620 in
Condition A
Industrial Laminates/Norplex NP631 Paper Base Laminate
Description: Hot punching grade with excellent electrical properties and low moisture absorption.Thickness Tested: 0.062", 0.125" and 0.500"
Dielectric Breakdown 60000 V

@Thickness 1.57 mm
60000 V

@Thickness 0.0620 in
Cond A; ASTM D229 S/S
Industrial Laminates/Norplex NP664 Paper Base Laminate
Description: Low cost room temperature punching grade with mechanical and electrical properties similar to NP612. This version is made with pigment cover plies on the surface.Thickness Tested: 0.062..