Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 10000 - 1.00e+20 ohm-cm | 10000 - 1.00e+20 ohm-cm | Average value: 5.21e+18 ohm-cm Grade Count:20 |
Overview of materials for High Density Polyethylene (HDPE), Extruded This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Extruded". Each property range of values reported is minimum and maxim.. |