Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0000490 ohm-cm | 0.0000490 ohm-cm | |
Indium Corp. Indalloy 140 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Electrical Resistivity | 0.0000490 ohm-cm | 0.0000490 ohm-cm | Temperature coefficient of resistance is 30 µOhm/Ohm-°C in the range 25-100°C. |
Special Metals FERRY® Alloy A copper-nickel alloy used mainly for its electrical properties. It has medium-range electrical resistivity and a very low temperature coefficient of resistance (TCR). The low TCR makes the alloy .. |
|||
Electrical Resistivity | 0.0000490 ohm-cm | 0.0000490 ohm-cm | |
CLAL-MSX ARCAP Anticorrosion AP4 H13 3/4 hard, Drawn Copper Alloy Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc.. |
|||
Electrical Resistivity | 0.0000490 ohm-cm | 0.0000490 ohm-cm | |
CLAL-MSX ARCAP Anticorrosion AP4 H14 4/4 hard, Drawn Copper Alloy Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc.. |
|||
Electrical Resistivity | 0.0000490 ohm-cm | 0.0000490 ohm-cm | |
CLAL-MSX ARCAP Anticorrosion AP4 H15 Spring, Drawn Copper Alloy Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc.. |
|||
Electrical Resistivity | 0.0000490 ohm-cm | 0.0000490 ohm-cm | |
CLAL-MSX ARCAP Anticorrosion AP4 H15 Spring, Rolled Copper Alloy Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc.. |
|||
Electrical Resistivity | 0.0000490 ohm-cm | 0.0000490 ohm-cm | |
CLAL-MSX ARCAP Anticorrosion AP4 0 Annealed, Drawn Copper Alloy Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc.. |
|||
Electrical Resistivity | 0.0000490 ohm-cm | 0.0000490 ohm-cm | |
CLAL-MSX ARCAP Anticorrosion AP4 0 Annealed, Rolled Copper Alloy Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc.. |
|||
Electrical Resistivity | 0.0000490 ohm-cm | 0.0000490 ohm-cm | |
CLAL-MSX ARCAP Anticorrosion AP4 H11 1/4 hard, Drawn Copper Alloy Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc.. |
|||
Electrical Resistivity | 0.0000490 ohm-cm | 0.0000490 ohm-cm | |
CLAL-MSX ARCAP Anticorrosion AP4 H11 1/4 hard, Rolled Copper Alloy Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc.. |
|||
Electrical Resistivity | 0.0000490 ohm-cm | 0.0000490 ohm-cm | |
CLAL-MSX ARCAP Anticorrosion AP4 H12 1/2 hard, Drawn Copper Alloy Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc.. |
|||
Electrical Resistivity | 0.0000490 ohm-cm | 0.0000490 ohm-cm | |
CLAL-MSX ARCAP Anticorrosion AP4 H12 1/2 hard, Rolled Copper Alloy Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc.. |
|||
Electrical Resistivity | 0.0000490 ohm-cm | 0.0000490 ohm-cm | |
Carpenter Chrome Core® 8 Alloy Data provided by Carpenter Technology Corporation.Chrome Core® alloys are a family of controlled chemistry, ferritic 8 and 12% chromium-iron alloys which are candidates for use in magnetic componen.. |
|||
Electrical Resistivity | 0.0000490 ohm-cm | 0.0000490 ohm-cm | |
Carpenter Kovar® Alloy (Glass and Ceramic Sealing Alloy) Data provided by Carpenter Technology Corporation.Kovar® alloy is a vacuum melted, Fe-Ni-Co, low expansion alloy whose chemical composition is controlled within narrow limits to assure precise unif.. |
|||
Electrical Resistivity | 0.0000490 ohm-cm @Temperature 20.0 °C |
0.0000490 ohm-cm @Temperature 68.0 °F |
|
Alloy Wire International RW 45 Ni-Cu Resistance Wire Used in thermocouples, power resistors, shunts, and wire wound precision restors up to 750°F (400°C)Information provided by Alloywire International. |
|||
Electrical Resistivity | 0.0000490 ohm-cm | 0.0000490 ohm-cm | |
Carpenter Chrome Core® 8-FM Alloy Data provided by Carpenter Technology Corporation.Chrome Core® alloys are a family of controlled chemistry, ferritic 8 and 12% chromium-iron alloys which are candidates for use in magnetic componen.. |