Electrical Properties Metric English Comments
Electrical Resistivity 0.0000490 ohm-cm
0.0000490 ohm-cm
Indium Corp. Indalloy 140 Bismuth Solder Alloy
Information Provided by Indium Corporation
Electrical Resistivity 0.0000490 ohm-cm
0.0000490 ohm-cm
Temperature coefficient of resistance is 30 µOhm/Ohm-°C in the range 25-100°C.
Special Metals FERRY® Alloy
A copper-nickel alloy used mainly for its electrical properties. It has medium-range electrical resistivity and a very low temperature coefficient of resistance (TCR). The low TCR makes the alloy ..
Electrical Resistivity 0.0000490 ohm-cm
0.0000490 ohm-cm
CLAL-MSX ARCAP Anticorrosion AP4 H13 3/4 hard, Drawn Copper Alloy
Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc..
Electrical Resistivity 0.0000490 ohm-cm
0.0000490 ohm-cm
CLAL-MSX ARCAP Anticorrosion AP4 H14 4/4 hard, Drawn Copper Alloy
Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc..
Electrical Resistivity 0.0000490 ohm-cm
0.0000490 ohm-cm
CLAL-MSX ARCAP Anticorrosion AP4 H15 Spring, Drawn Copper Alloy
Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc..
Electrical Resistivity 0.0000490 ohm-cm
0.0000490 ohm-cm
CLAL-MSX ARCAP Anticorrosion AP4 H15 Spring, Rolled Copper Alloy
Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc..
Electrical Resistivity 0.0000490 ohm-cm
0.0000490 ohm-cm
CLAL-MSX ARCAP Anticorrosion AP4 0 Annealed, Drawn Copper Alloy
Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc..
Electrical Resistivity 0.0000490 ohm-cm
0.0000490 ohm-cm
CLAL-MSX ARCAP Anticorrosion AP4 0 Annealed, Rolled Copper Alloy
Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc..
Electrical Resistivity 0.0000490 ohm-cm
0.0000490 ohm-cm
CLAL-MSX ARCAP Anticorrosion AP4 H11 1/4 hard, Drawn Copper Alloy
Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc..
Electrical Resistivity 0.0000490 ohm-cm
0.0000490 ohm-cm
CLAL-MSX ARCAP Anticorrosion AP4 H11 1/4 hard, Rolled Copper Alloy
Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc..
Electrical Resistivity 0.0000490 ohm-cm
0.0000490 ohm-cm
CLAL-MSX ARCAP Anticorrosion AP4 H12 1/2 hard, Drawn Copper Alloy
Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc..
Electrical Resistivity 0.0000490 ohm-cm
0.0000490 ohm-cm
CLAL-MSX ARCAP Anticorrosion AP4 H12 1/2 hard, Rolled Copper Alloy
Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc..
Electrical Resistivity 0.0000490 ohm-cm
0.0000490 ohm-cm
Carpenter Chrome Core® 8 Alloy
Data provided by Carpenter Technology Corporation.Chrome Core® alloys are a family of controlled chemistry, ferritic 8 and 12% chromium-iron alloys which are candidates for use in magnetic componen..
Electrical Resistivity 0.0000490 ohm-cm
0.0000490 ohm-cm
Carpenter Kovar® Alloy (Glass and Ceramic Sealing Alloy)
Data provided by Carpenter Technology Corporation.Kovar® alloy is a vacuum melted, Fe-Ni-Co, low expansion alloy whose chemical composition is controlled within narrow limits to assure precise unif..
Electrical Resistivity 0.0000490 ohm-cm

@Temperature 20.0 °C
0.0000490 ohm-cm

@Temperature 68.0 °F
Alloy Wire International RW 45 Ni-Cu Resistance Wire
Used in thermocouples, power resistors, shunts, and wire wound precision restors up to 750°F (400°C)Information provided by Alloywire International.
Electrical Resistivity 0.0000490 ohm-cm
0.0000490 ohm-cm
Carpenter Chrome Core® 8-FM Alloy
Data provided by Carpenter Technology Corporation.Chrome Core® alloys are a family of controlled chemistry, ferritic 8 and 12% chromium-iron alloys which are candidates for use in magnetic componen..