Electrical Resistivity 0.0000200 ohm-cm
0.0000200 ohm-cm
Indium Corp. Indalloy 161 Lead Solder Alloy
Torch solder, poor corrosion resistanceInformation Provided by Indium Corporation
Electrical Resistivity 0.0000200 ohm-cm
0.0000200 ohm-cm
Indium Corp. Indalloy® 151 Pb-Sn-Ag Solder Alloy
Similar to Indalloy #165 (Standard lead-silver-tin eutectic solder with wide application in semiconductor assembly.)Information provided by the manufacturer, Indium Corporation.
Electrical Resistivity 0.0000200 ohm-cm
0.0000200 ohm-cm
Indium Corp. Indalloy® 204 In-Pb Solder Alloy
Indalloy's #7, #10, #150, #204, #205 and #206 comprise a group of lead-indium solders designed to cover the temperature range of 165°C-275°C. All have the minimum gold-leaching characteristics..
Electrical Resistivity 0.0000200 ohm-cm
0.0000200 ohm-cm
Indium Corp. Indalloy® 228 Pb-Sn-Ag Solder Alloy
(Sn10) High temp solder. Not recommended for applications above 120°C, due to formation of eutectic.Information provided by the manufacturer, Indium Corporation.
Electrical Resistivity 0.0000200 ohm-cm
0.0000200 ohm-cm
Indium Corp. Indalloy® 171 Pb-Sn Solder Alloy
Wide application in soldering.Information provided by the manufacturer, Indium Corporation.