Material Notes:
Similar to Indalloy #165 (Standard lead-silver-tin eutectic solder with wide application in semiconductor assembly.)Information provided by the manufacturer, Indium Corporation.
Physical Properties Metric English Comments
Density 11.02 g/cc
0.3981 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 29.0 MPa
4210 psi
Modulus of Elasticity 13.8 GPa
2000 ksi
Shear Strength 15.4 MPa
2230 psi
Shear Bond Holding Strength
Thermal Properties Metric English Comments
CTE, linear 29.0 µm/m-°C

@Temperature 20.0 °C
16.1 µin/in-°F

@Temperature 68.0 °F
Specific Heat Capacity 0.130 J/g-°C
0.0311 BTU/lb-°F
Solid
Melting Point 287 - 296 °C
549 - 565 °F
Solidus 287 °C
549 °F
Liquidus 296 °C
565 °F
Component Elements Properties Metric English Comments
Lead, Pb 92.5 %
92.5 %
Silver, Ag 2.5 %
2.5 %
Tin, Sn 5.0 %
5.0 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000200 ohm-cm
0.0000200 ohm-cm