Indium Corp. Indalloy® 171 Pb-Sn Solder Alloy

Category Metal , Nonferrous Metal , Lead Alloy , Solder/Braze Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy® 171 Pb-Sn Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Wide application in soldering.Information provided by the manufacturer, Indium Corporation.
Physical Properties Metric English Comments
Density 11.06 g/cc
0.3996 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 8.0

@Load 100 kg,
Time 30.0 sec
8.0

@Load 220 lb,
Time 0.00833 hour
Tensile Strength, Ultimate 27.6 MPa
4000 psi
Elongation at Break 45 %
45 %
Shear Strength 14.5 MPa
2100 psi
Shear Bond Holding Strength
Thermal Properties Metric English Comments
CTE, linear 30.0 µm/m-°C

@Temperature 20.0 °C
16.7 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 23.0 W/m-K

@Temperature 85.0 °C
160 BTU-in/hr-ft²-°F

@Temperature 185 °F
Melting Point 308 - 312 °C
586 - 594 °F
Solidus 308 °C
586 °F
Liquidus 312 °C
594 °F
Component Elements Properties Metric English Comments
Lead, Pb 95 %
95 %
Tin, Sn 5.0 %
5.0 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000200 ohm-cm
0.0000200 ohm-cm