Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | <= 0.00000780 ohm-cm | <= 0.00000780 ohm-cm | |
IBC Advanced Alloys C17510 Beryllium Copper Alloy Rounds, Temper AT(TF00) C17510 - Beryllium Copper mold alloys have hardnesses comparable to tool steel, but with superior thermal conductivity. Beryllium copper plate, block, bar and rounds -- upset forged and heat treated.. |
|||
Electrical Resistivity | 0.00000780 ohm-cm | 0.00000780 ohm-cm | |
Indium Corp. Indalloy® 3 In-Ag Solder Alloy Has nearly the wettability and low temperature malleability of Indium. Solders silver, fired glass, and ceramics. Large plastic range.Information provided by the manufacturer, Indium Corporation. |
|||
Electrical Resistivity | 0.00000780 ohm-cm | 0.00000780 ohm-cm | quenched |
CLAL-MSX SICLANIC S® TB Quenched Copper Alloy SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver.. |
|||
Electrical Resistivity | 0.00000780 ohm-cm | 0.00000780 ohm-cm | quenched |
CLAL-MSX SICLANIC S® TD4 Quenched Copper Alloy, 4/4 Hard SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver.. |
|||
Electrical Resistivity | 0.00000780 ohm-cm | 0.00000780 ohm-cm | quenched |
CLAL-MSX SICLANIC S® TF Quenched Copper Alloy, precipitation treated SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver.. |
|||
Electrical Resistivity | 0.00000780 ohm-cm | 0.00000780 ohm-cm | quenched |
CLAL-MSX SICLANIC S® TH3 Quenched Copper Alloy, 1/2 Hard, precipitation treated SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver.. |
|||
Electrical Resistivity | 0.00000780 ohm-cm | 0.00000780 ohm-cm | quenched |
CLAL-MSX SICLANIC S® TH4 Quenched Copper Alloy, 4/4 Hard, precipitation treated SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver.. |
|||
Electrical Resistivity | 0.00000780 ohm-cm | 0.00000780 ohm-cm | Drawn Rod & Bar (22% IACS) |
CMW® 73 Copper Alloy CMW® 73 material is a heat treatable copper base alloy having extremely high hardness and strength coupled with fair electrical and thermal conductivity. The extremely high hardness, strength and w.. |
|||
Electrical Resistivity | 0.00000780 ohm-cm | 0.00000780 ohm-cm | quenched |
CLAL-MSX SICLANIC S® TD3 Quenched Copper Alloy, 1/2 Hard SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver.. |