Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00000615 ohm-cm | 0.00000615 ohm-cm | |
Chicago Extruded Metals UNS C38500 Copper-Zinc-Lead Alloy Copper-Zinc-Lead Alloy (Leaded Brass)Finished product available in shapes.Chicago Extruded Metal temper codes: H01, H02Information provided by Chicago Extruded Metals |
|||
Electrical Resistivity | 0.00000615 ohm-cm | 0.00000615 ohm-cm | 3% tolerance on sizes below 0.02, 5% tolerance on sizes above 0.02 |
California Fine Wire Alloy 411 Precious Metal Alloy All values may vary dependent on specific design and usageProprietary compositionCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |