Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

California Fine Wire Alloy 411 Precious Metal Alloy

Category Metal , Nonferrous Metal
Manufacturer California Fine Wire
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF California Fine Wire Alloy 411 Precious Metal Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
All values may vary dependent on specific design and usageProprietary compositionCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Physical Properties Metric English Comments
Density 10.9 g/cc
0.393 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break 407 MPa
59000 psi
Stress relieved
493 MPa
71500 psi
Hard
Modulus of Elasticity 32.5 GPa
4710 ksi
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000615 ohm-cm
0.00000615 ohm-cm
3% tolerance on sizes below 0.02, 5% tolerance on sizes above 0.02
Descriptive Properties Value Comments
Magnetic None
Temperature Coefficient of Resistance 0.0008 ohms/ohm-°C
0-100°C
Thermal EMF vs. Copper -0.0019
Copyright © lookpolymers.com All Rights Reserved