Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chicago Extruded Metals UNS C38500 Copper-Zinc-Lead Alloy

Category Metal , Nonferrous Metal , Copper Alloy , Brass
Manufacturer Chicago Extruded Metals (CXM)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chicago Extruded Metals UNS C38500 Copper-Zinc-Lead Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Copper-Zinc-Lead Alloy (Leaded Brass)Finished product available in shapes.Chicago Extruded Metal temper codes: H01, H02Information provided by Chicago Extruded Metals
Physical Properties Metric English Comments
Density 8.47 g/cc
0.306 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 65
65
Tensile Strength 414 MPa
60000 psi
Tensile Strength, Yield 138 MPa
20000 psi
Elongation at Break 30 %
30 %
Machinability 90 %
90 %
UNS C36000 (free-cutting brass) = 100%
Thermal Properties Metric English Comments
Thermal Conductivity 123 W/m-K
852 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Copper, Cu 55 - 59 %
55 - 59 %
Iron, Fe 0.35 %
0.35 %
Lead, Pb 2.5 - 3.5 %
2.5 - 3.5 %
Other, total 0.50 %
0.50 %
Zinc, Zn 36.65 - 41.65 %
36.65 - 41.65 %
as balance
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000615 ohm-cm
0.00000615 ohm-cm
Copyright © lookpolymers.com All Rights Reserved