Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00000480 - 0.00000500 ohm-cm | 0.00000480 - 0.00000500 ohm-cm | |
PEAK Werkstoff DISPAL S690 Aluminum Alloy, AlCu4MgAg, Condition T4 High stiffness and elongation at rupture. Property data for Condition T4 (Quench in water at RT).Information provided by PEAK Werkstoff GmbH |
|||
Electrical Resistivity | 0.00000480 - 0.00000500 ohm-cm | 0.00000480 - 0.00000500 ohm-cm | |
PEAK Werkstoff DISPAL S690 Aluminum Alloy, AlCu4MgAg, Condition T6 High stiffness and elongation at rupture. Property data for Condition T6 (Quench in water at RT).Information provided by PEAK Werkstoff GmbH |