Material Notes:
High stiffness and elongation at rupture. Property data for Condition T6 (Quench in water at RT).Information provided by PEAK Werkstoff GmbH
Physical Properties Metric English Comments
Density 2.66 - 2.94 g/cc
0.0961 - 0.106 lb/in³
Mechanical Properties Metric English Comments
Hardness, Vickers >= 135
>= 135
HV30
Tensile Strength at Break >= 520 MPa
>= 75400 psi
Tensile Strength, Yield >= 430 MPa
>= 62400 psi
Elongation at Break >= 11.7 %
>= 11.7 %
Modulus of Elasticity >= 72.0 GPa
>= 10400 ksi
Thermal Properties Metric English Comments
CTE, linear 22.9 - 23.9 µm/m-°C

@Temperature 20.0 - 100 °C
12.7 - 13.3 µin/in-°F

@Temperature 68.0 - 212 °F
23.6 - 24.6 µm/m-°C

@Temperature 20.0 - 200 °C
13.1 - 13.7 µin/in-°F

@Temperature 68.0 - 392 °F
24.6 - 25.6 µm/m-°C

@Temperature 20.0 - 300 °C
13.7 - 14.2 µin/in-°F

@Temperature 68.0 - 572 °F
Melting Point 549 - 664 °C
1020 - 1230 °F
Solidus 548.7 - 554.7 °C
1020 - 1030 °F
Liquidus 657.3 - 663.9 °C
1215 - 1227 °F
Component Elements Properties Metric English Comments
Aluminum, Al 94 %
94 %
As Balance
Copper, Cu 4.0 %
4.0 %
Magnesium, Mg 1.0 %
1.0 %
Silver, Ag 1.0 %
1.0 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000480 - 0.00000500 ohm-cm
0.00000480 - 0.00000500 ohm-cm