Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00000480 - 0.00000500 ohm-cm | 0.00000480 - 0.00000500 ohm-cm | |
PEAK Werkstoff DISPAL S690 Aluminum Alloy, AlCu4MgAg, Condition T4 High stiffness and elongation at rupture. Property data for Condition T4 (Quench in water at RT).Information provided by PEAK Werkstoff GmbH |
|||
Electrical Resistivity | 0.00000480 - 0.00000500 ohm-cm | 0.00000480 - 0.00000500 ohm-cm | |
PEAK Werkstoff DISPAL S690 Aluminum Alloy, AlCu4MgAg, Condition T6 High stiffness and elongation at rupture. Property data for Condition T6 (Quench in water at RT).Information provided by PEAK Werkstoff GmbH |
|||
Electrical Resistivity | 0.00000480 - 0.00000590 ohm-cm | 0.00000480 - 0.00000590 ohm-cm | Temper T651 |
Constellium ALPLAN® 7075 High-Strength Rolled Precision Aluminum Plate, Milled Both Sides ALPLAN® 7075 precision plates combine a good dimensional stability with high mechanical strength. Both the outstanding flatness and the low roughness of the surfaces, protected by a plastic film, m.. |
|||
Electrical Resistivity | 0.00000480 ohm-cm | 0.00000480 ohm-cm | precipitation hardened (1 hr) |
CLAL-MSX SICLANIC S® TH4 Quenched Copper Alloy, 4/4 Hard, precipitation treated SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver.. |