Electrical Properties Metric English Comments
Electrical Resistivity 0.00000490 - 0.00000860 ohm-cm
0.00000490 - 0.00000860 ohm-cm
20-35% IACS Conductivity
Materion Beryllium Copper Alloy 3 Forgings & Extrusions; A (TB00) Temper (UNS C17510)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Electrical Resistivity 0.00000490 - 0.00000860 ohm-cm
0.00000490 - 0.00000860 ohm-cm
20-35% IACS Conductivity
Materion Beryllium Copper Alloy 10 Forgings & Extrusions; A (TB00) Temper (UNS C17500)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Electrical Resistivity 0.00000490 ohm-cm
0.00000490 ohm-cm
Alcoa Deltalloy® 4032-T86 Aluminum
Weldability = B; Stress Corrosion Cracking Resistance = B; General Corrosion Resistance = C (A = best; E = worst). General 4032 characteristics and uses: Good machinability and drilling characterist..
Electrical Resistivity 0.00000490 ohm-cm
0.00000490 ohm-cm
Alcoa Excalibar® 6013-T651 Aluminum
Alcoa recommends as a higher machinability alternative to 6061-T651. It has the potential for higher machining speeds and feed rates, easier deburring,ease of clearing 'chips' and better finishes. ..
Electrical Resistivity 0.00000490 ohm-cm
0.00000490 ohm-cm
ECOMold 95 Copper Mold Material
ECOMold® copper alloys (beryllium-free) are designed specifically for plastics industry applications. ECOMold® 95 has a superior combination of thermal conductivity, hardness, and tensile strengt..
Electrical Resistivity 0.00000490 ohm-cm
0.00000490 ohm-cm
precipitation hardened (1 hr)
CLAL-MSX SICLANIC S® TF Quenched Copper Alloy, precipitation treated
SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver..
Electrical Resistivity 0.00000490 ohm-cm
0.00000490 ohm-cm
35 % IACS
CMW® ELKONITE 2088 very high refractory, tungsten, silver
ELKONITE® 2088 has a very high refractory content and is not considered in the normal family of make and break contacts. It is used in special applications where weight or hardness together with co..
Electrical Resistivity 0.00000490 ohm-cm
0.00000490 ohm-cm
35 % IACS
CMW® ELKONIUM 217 Silver Cadmium Alloy
The alloying of silver with cadmium produces materials with good arc extinction, good corrosion resistance and low contact resistance characteristics and provides them with good switching capability..