Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00000400 - 0.00000520 ohm-cm | 0.00000400 - 0.00000520 ohm-cm | |
Constellium PLAN 5754 Aluminum Rolled Plate Rolled plates in 5754 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 5754 PLAN is mainly used for low stressed mechanical components, manufactured by intensive m.. |
|||
Electrical Resistivity | 0.00000400 - 0.00000520 ohm-cm | 0.00000400 - 0.00000520 ohm-cm | |
Constellium PLAN OX 5754 Aluminum Rolled Plate Rolled plates in 5754 PLAN OX are optimized for minimum residual stress, improved dimensional tolerances and for decorative* anodizing. 5754 PLAN OX is mainly used for low stressed, anodized compone.. |
|||
Electrical Resistivity | <= 0.00000400 ohm-cm | <= 0.00000400 ohm-cm | precipitation hardened |
CLAL-MSX SICLANIC S® TB Quenched Copper Alloy SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver.. |
|||
Electrical Resistivity | 0.00000400 ohm-cm | 0.00000400 ohm-cm | precipitation hardened (4 hr) |
CLAL-MSX SICLANIC S® TB Quenched Copper Alloy SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver.. |
|||
Electrical Resistivity | <= 0.00000400 ohm-cm | <= 0.00000400 ohm-cm | precipitation hardened |
CLAL-MSX SICLANIC S® TD4 Quenched Copper Alloy, 4/4 Hard SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver.. |
|||
Electrical Resistivity | <= 0.00000400 ohm-cm | <= 0.00000400 ohm-cm | precipitation hardened |
CLAL-MSX SICLANIC S® TF Quenched Copper Alloy, precipitation treated SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver.. |
|||
Electrical Resistivity | <= 0.00000400 ohm-cm | <= 0.00000400 ohm-cm | precipitation hardened |
CLAL-MSX SICLANIC S® TH3 Quenched Copper Alloy, 1/2 Hard, precipitation treated SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver.. |
|||
Electrical Resistivity | <= 0.00000400 ohm-cm | <= 0.00000400 ohm-cm | precipitation hardened |
CLAL-MSX SICLANIC S® TH4 Quenched Copper Alloy, 4/4 Hard, precipitation treated SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver.. |
|||
Electrical Resistivity | <= 0.00000400 ohm-cm | <= 0.00000400 ohm-cm | precipitation hardened |
CLAL-MSX SICLANIC S® TD3 Quenched Copper Alloy, 1/2 Hard SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver.. |
|||
Electrical Resistivity | 0.00000400 ohm-cm | 0.00000400 ohm-cm | 43 % IACS |
CMW® ELKONIUM 18 silver, copper, cadmium alloy The alloying of silver with cadmium produces materials with good arc extinction, good corrosion resistance and low contact resistance characteristics and provides them with good switching capability.. |