Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00000391 ohm-cm | 0.00000391 ohm-cm | |
Chicago Extruded Metals BioBrass® UNS C22000 Copper-Zinc Alloy Finished product available as bar or wire.Chicago Extruded Metal temper codes: H01, H02, H04This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Extruded Metal.. |
|||
Electrical Resistivity | 0.00000391 - 0.00000453 ohm-cm | 0.00000391 - 0.00000453 ohm-cm | Calculated from 38-44 %IACS |
Cadi 10TC Tungsten Carbide Copper Available in a variety of rounds, rectangles, and shapes.Information provided by Cadi Company. |