Polymer Property : Electrical Resistivity = 0.00000391 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000391 ohm-cm
0.00000391 ohm-cm
Chicago Extruded Metals BioBrass® UNS C22000 Copper-Zinc Alloy
Finished product available as bar or wire.Chicago Extruded Metal temper codes: H01, H02, H04This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Extruded Metal..
Electrical Resistivity 0.00000391 - 0.00000453 ohm-cm
0.00000391 - 0.00000453 ohm-cm
Calculated from 38-44 %IACS
Cadi 10TC Tungsten Carbide Copper
Available in a variety of rounds, rectangles, and shapes.Information provided by Cadi Company.