Polymer Property : Electrical Resistivity = 0.00000277 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000246 - 0.00000277 ohm-cm
0.00000246 - 0.00000277 ohm-cm
Calculated from 62-70 %IACS
Cadi 50WS Tungsten Silver
Available in a variety of rounds, rectangles, and shapes.Information provided by Cadi Company.