Cadi 50WS Tungsten Silver

Category Metal , Metal Matrix Composite , Nonferrous Metal , Precious Metal , Silver Alloy , Refractory Metal , Tungsten Alloy
Manufacturer Cadi Company
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cadi 50WS Tungsten Silver.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Available in a variety of rounds, rectangles, and shapes.Information provided by Cadi Company.
Physical Properties Metric English Comments
Density 13.48 g/cc
0.4870 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 50 - 60
50 - 60
Component Elements Properties Metric English Comments
Silver, Ag 50 %
50 %
Tungsten, W 50 %
50 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000246 - 0.00000277 ohm-cm
0.00000246 - 0.00000277 ohm-cm
Calculated from 62-70 %IACS