Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00000246 ohm-cm | 0.00000246 ohm-cm | (70% IACS) |
CMW® D55X Post-oxidized Silver Cadmium Oxide Contact Material ASTM B781, Table 3 For electrical contacts; resistant to welding and high surge currentsInformation provided by CMW Inc. |
|||
Electrical Resistivity | 0.00000246 - 0.00000277 ohm-cm | 0.00000246 - 0.00000277 ohm-cm | Calculated from 62-70 %IACS |
Cadi 50WS Tungsten Silver Available in a variety of rounds, rectangles, and shapes.Information provided by Cadi Company. |