Electrical Properties Metric English Comments
Electrical Resistivity 0.00000200 - 0.00000400 ohm-cm
0.00000200 - 0.00000400 ohm-cm
In-Plane; ASTM-C611
GrafTech GRAFCELL® GDB Graphite Gas Diffusion Barrier
GRAFCELL® Gas Diffusion Barrier (GDB) material is a thin, perforated structure made from a continuous matrix of expanded natural graphite with excellent electrical conductivity, thermal conductiv..