Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Hot Wire Ignition, HWI = 14 sec Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Hot Wire Ignition, HWI 14 - 29 sec

@Thickness 3.00 mm
14 - 29 sec

@Thickness 0.118 in
UL 746
Ascend Performance Materials Vydyne® 49 Nylon 66, Impact Modified, DAM
Vydyne® 49 is general-purpose, impact-modified PA66 resin. Available in natural, is recognized for all the processing and property advantages inherent to PA66 with the addition of improved impact s..
Hot Wire Ignition, HWI 14 - 29 sec

@Thickness 3.00 mm
14 - 29 sec

@Thickness 0.118 in
UL 746
Ascend Performance Materials Vydyne® 49H NT Nylon 66, Impact Modified, DAM
Vydyne® 49H NT is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat-stabilized for improved resista..