Electrical Properties | Metric | English | Comments |
---|---|---|---|
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 1.50 mm |
15 - 29 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® 20NSP Nylon 66, DAM Vydyne® 20NSP is a general-purpose, highly nucleated, lubricated PA66 resin available in natural color. It is designed to crystallize rapidly in order to reduce cycle times and increase productivit.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 1.50 mm |
15 - 29 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® 20NSP1 Nylon 66, DAM Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 43% Filler by Weight Additive:Nucleating AgentLubricant Features:Fast Molding CycleGeneral PurposeGood Mold Release Good.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 1.50 mm |
15 - 29 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® 21SPC1 Nylon 66, DAM Vydyne® 21SPC1 is a general-purpose, improved-flow, lubricated PA66 resin available in natural color. 21SPC1 offers a balanced combination of properties characterized by high strength, rigidity, go.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 1.50 mm |
15 - 29 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® 21SPF BLK Nylon 66, Conditioned Vydyne® 21SPF BLK is a, general-purpose PA66 resin used for extrusion-compounding. Available in black, it is designed principally for injection-molding fabrication. This grade offers a well-balance.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 3.00 mm |
15 - 29 sec @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® 21SPF BLK Nylon 66, Conditioned Vydyne® 21SPF BLK is a, general-purpose PA66 resin used for extrusion-compounding. Available in black, it is designed principally for injection-molding fabrication. This grade offers a well-balance.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 1.50 mm |
15 - 29 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® 21SPG1 Nylon 66, DAM Availability:Asia PacificEuropeNorth America Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood ToughnessHigh Rigidit.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 3.00 mm |
15 - 29 sec @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® 21SPG1 Nylon 66, DAM Availability:Asia PacificEuropeNorth America Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood ToughnessHigh Rigidit.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 3.00 mm |
15 - 29 sec @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® 47H BK0501 Nylon 66, Impact Modified, DAM Vydyne® 47H BK0501 is general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 3.00 mm |
15 - 29 sec @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® 47H BK0668 Nylon 66, Impact Modified, Heat Stabilized, DAM Vydyne® 47H BK0668 is a high-performance, medium-impact-modified, heat-stabilized grade of PA66 resin.Availability:Asia PacificEuropeNorth AmericaAdditive:Impact Modifier Features:Gasoline Resistan.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 3.00 mm |
15 - 29 sec @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® 49 Nylon 66, DAM Vydyne® 49 is a general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved imp.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 3.00 mm |
15 - 29 sec @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® ECO315 BK06 Nylon 66/6, Flame Retardant, DAM Vydyne® ECO315 BK06 is a non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent toughness and ductility. It is lubricated for machine feed and easy mold release and has Underwri.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 1.50 mm |
15 - 29 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® R513H Black Nylon 66, 13% Glass Reinforced, DAM Vydyne® R513H Black is general-purpose, 13% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is an injection-molding grade that is lubricated for machine feed, flow, and m.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 1.50 mm |
15 - 29 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® R525H BK02 Nylon 66, 25% Glass Reinforced, DAM Vydyne® R525H BK02 is high-flow, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 1.50 mm |
15 - 29 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® R530H BK0201 Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530H BK0201 is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in black, it is specifically designed to maximize the retention of p.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 1.50 mm |
15 - 29 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® R530H BK0202 Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530H BK0202 is general-purpose, recycled, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in black, it is specifically designed to maximize the rete.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 1.50 mm |
15 - 29 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® R533H NT Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H NT is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties .. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 1.50 mm |
15 - 29 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® R540H Nylon 66, 40% Glass Reinforced, DAM Vydyne® R540H is general-purpose, heat-stabilized, hydrolysis-resistant, 40% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physic.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 1.50 mm |
15 - 29 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® R543H BK02 Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H BK02 is general-purpose, 43% glass-fiber reinforced PA66 resin. Available in black, it is an injection-molding grade resin that is lubricated for machine feed, flow and mold release. .. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 1.50 mm |
15 - 29 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® R543H Natural Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H Natural is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fe.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 1.50 mm |
15 - 29 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® R543H NT Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H NT is general-purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine feed, flow and mold release. .. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 3.00 mm |
15 - 29 sec @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® 41 Nylon 66, DAM Vydyne® 41 is a general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved imp.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 3.00 mm |
15 - 29 sec @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® 41H NT Nylon 66, Impact Modified, DAM Vydyne® 41H NT is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyn.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 3.00 mm |
15 - 29 sec @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® 47H BK0644 Nylon 66, Impact Modified, DAM Vydyne® 47H BK0644 is a high-performance, medium-impact-modified, heat-stabilized PA66 resin with excellent UV stability and outstanding processing characteristics. This product has an UL746C f1 ra.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 3.00 mm |
15 - 29 sec @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® 64C-R Nylon 66, DAM Vydyne® 64C-R is a medium-viscosity PA66 resin suitable for injection-molding, extrusion and compounding applications. It is available in natural color only. Vydyne 64C-R resin offers high strength.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 1.50 mm |
15 - 29 sec @Thickness 0.0591 in |
UL 746A |
Ascend Performance Materials Vydyne® 66B Nylon 66, General Purpose, high viscosity, DAM Vydyne® 66B is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66B resin offers high strength, .. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 1.50 mm |
15 - 29 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® 20NSP1 Nylon 66, DAM Availability:Asia PacificEuropeNorth AmericaAdditive:LubricantNucleating Agent Features: Fast Molding CycleGeneral PurposeGood Mold ReleaseGood StiffnessHigh RigidityLubricatedNucleatedUses:Bearings.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 3.00 mm |
15 - 29 sec @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® 41 NT Nylon 66, Impact Modified, DAM Vydyne® 41 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 1.50 mm |
15 - 29 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® ECO366 Nylon 66, Flame-retardant, DAM Vydyne® ECO366 is a non-halogenated, unfilled, flame-retardant PA66 homopolymer designed with superior flow properties to assist in filling thin-walled, intricate parts. It is lubricated for machin.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 1.50 mm |
15 - 29 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® R533H NAT Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H NAT is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 1.50 mm |
15 - 29 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® 22HSP NT Nylon 66, DAM Availability:Asia PacificEuropeNorth AmericaAdditive: Lubricant Features:Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood Tou.. |