Polymer Property : Melt Temperature = 534 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 149 - 279 °C
300 - 534 °F
Average value: 219 °C Grade Count:177
Overview of materials for Polypropylene with 20% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Talc Filler".Specific grades with primary filler content between 15% and 24% are ..
Melt Temperature 170 - 279 °C
338 - 534 °F
Average value: 222 °C Grade Count:70
Overview of materials for Polypropylene with 30% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Talc Filler". Specific grades with primary filler content between 25% and 34% are..
Melt Temperature 170 - 279 °C
338 - 534 °F
Average value: 217 °C Grade Count:15
Overview of materials for Polypropylene with 40% Calcium Carbonate (CaCO3) Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be..
Melt Temperature 241 - 279 °C
466 - 534 °F
Injection
Albis Plastics ASA 02A 811 Unreinforced  (discontinued **)
Acrylonitrile/Styrene/AcrylateCharacteristics: Excellent UV, Good Rigidity, Good Dimensional StabilityApplications: Sunglasses, Boat Shells, Roofs for Campers & RVsProcessing: Injection Molding (Mel..
Melt Temperature 241 - 279 °C
466 - 534 °F
Injection Molding
Styrolution Luran® S 778 T ASA
Luran S 778 T is an injection molding ASA grade with enhanced toughness and heat resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS.
Melt Temperature 241 - 279 °C
466 - 534 °F
Injection
Albis Plastics ASA 02A MR20 , 20% Mineral Filled  (discontinued **)
Acrylonitrile/Styrene/AcrylateCharacteristics: Excellent UV, Good Rigidity, Good Dimensional StabilityApplications: Sunglasses, Boat Shells, Roofs for Campers & RVsProcessing: Injection Molding (Mel..
Melt Temperature 170 - 279 °C
338 - 534 °F
Average value: 215 °C Grade Count:51
Overview of materials for Polypropylene with 10% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Talc Filler". Specific grades with primary filler content between 5% and 14% are ..
Melt Temperature 170 - 279 °C
338 - 534 °F
Average value: 224 °C Grade Count:92
Overview of materials for Polypropylene with 40% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Talc Filler". Specific grades with primary filler content between 35% and 44% are..
Melt Temperature 170 - 279 °C
338 - 534 °F
Average value: 205 °C Grade Count:6
Overview of materials for Polypropylene with 10% Calcium Carbonate (CaCO3) Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be..