DuPont Performance Polymers Crastin® S610SF BK851 PBT  (Unverified Data**)

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Crastin® S610SF BK851 PBT  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Crastin® S610SF is an unreinforced, low viscosity polybutylene terephthalate for injection molding. It has high flow characteristics and is specifically suitable for super fast production.Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.32 g/cc
0.0477 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.017 cm/cm

@Thickness 2.00 mm
0.017 in/in

@Thickness 0.0787 in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.016 cm/cm

@Thickness 2.00 mm
0.016 in/in

@Thickness 0.0787 in
ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength, Yield 60.0 MPa

@Temperature 23.0 °C
8700 psi

@Temperature 73.4 °F
ISO 527
Elongation at Break 13 %

@Temperature 23.0 °C
13 %

@Temperature 73.4 °F
nominal; ISO 527
Elongation at Yield 10 %

@Temperature 23.0 °C
10 %

@Temperature 73.4 °F
ISO 527
Tensile Modulus 2.60 GPa

@Temperature 23.0 °C
377 ksi

@Temperature 73.4 °F
ISO 527
Charpy Impact, Notched 0.400 J/cm²

@Temperature 23.0 °C
1.90 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 224 °C
435 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 54.0 °C
129 °F
ISO 75-1/-2
Processing Properties Metric English Comments
Melt Temperature 240 °C
464 °F
Optimum
235 - 260 °C
455 - 500 °F
Mold Temperature 80.0 °C
176 °F
optimum
30.0 - 130 °C
86.0 - 266 °F
Drying Temperature 110 - 130 °C
230 - 266 °F
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
Moisture Content <= 0.040 %
<= 0.040 %
Descriptive Properties Value Comments
Appearance Black Color
Features High productivity
Forms Pellets
Generic PBT
Material Status Preliminary Data
Part Marking Code >PBT<
ISO 11469
Processing Method Injection Molding
Injection Molding
Injection Molding
Injection Molding
Product Category Fast Cycle Resins
Fast Cycle Resins
Unreinforced Resins
Region Available - Global Yes
Resin Identification PBT
ISO 1043
RoHS Compliance Contact Manufacturer
Uses Automotive Applications
Fibers