Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 202 - 218 °C | 396 - 424 °F | |
NatureWorks® Ingeo™ 4032D Film Grade PLA NatureWorks® PLA (polylactide) polymer 4032D can be converted into a biaxially oriented film with use temperatures up to 300°F (150°C). This film has excellent optics, good machinability and exce.. |
|||
Melt Temperature | 202 - 218 °C | 396 - 424 °F | |
NatureWorks® Ingeo™ 4043D General Purpose Film Grade Biopolymer Ingeo 4043D can be converted into a biaxially oriented film with use temperatures up to 265ºF (130ºC). This film has excellent optics, good machinability and excellent twist and deadfold. These pr.. |
|||
Melt Temperature | 202 - 210 °C | 396 - 410 °F | |
PolyOne Geon™ HTX M6215 Polyvinyl Chloride Alloy (PVC Alloy) It is recommended that the compound pellets be dried for 3 to 4 hours at 150 deg. F.Information provided by PolyOne |
|||
Melt Temperature | 202 - 207 °C | 396 - 405 °F | |
PolyOne Geon™ HTX M6307 Polyvinyl Chloride Alloy (PVC Alloy) Information provided by PolyOne |
|||
Melt Temperature | 202 - 250 °C | 396 - 482 °F | Average value: 226 °C Grade Count:14 |
Overview of materials for Cellulose Acetate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate, Molded". Each property range of values reported is minimum and maximum values of appr.. |
|||
Melt Temperature | 202 °C | 396 °F | Injection Molding |
Albis Plastics Cellulose Acetate CA700 , Unreinforced, 37% Plasticizer
(discontinued **) Amorphous Cellulose Acetate (CA)Characteristics: Chemical Resistance, Toughness, Strength, Hardness, Gloss, Clarity and "Feel"Applications: Tool Handles, Optical Products, Toys and Sheet ProductsPro.. |
|||
Melt Temperature | 202 °C | 396 °F | Injection |
Albis Plastics Cellulose Acetate Butyrate B900 (Base Grade), 20% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Melt Temperature | 202 °C | 396 °F | Injection |
Albis Plastics Cellulose Acetate Butyrate B902 (UV Inhibitor Added), 20% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Melt Temperature | 202 °C | 396 °F | Injection |
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 20% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Melt Temperature | 202 °C | 396 °F | Injection |
Albis Plastics Cellulose Acetate Butyrate B9024 (UVI, Odor Mask Added), 20% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |