Processing Properties Metric English Comments
Melt Temperature 370 - 395 °C
698 - 743 °F
Parker Chomerics PREMIER™ PEI-140 High Temperature Conductive Plastic for EMI Shielding
PEI-140 can provide up to a 65% cost reduction by eliminating secondary operations such as assembly, machining, painting/plating and the logistics that accompany these processes. The shielding effec..
Melt Temperature 370 - 390 °C
698 - 734 °F
LATI LARPEEK 10 G/50 50% Glass Reinforced Polyetheretherketone (PEEK)  (Unverified Data**)
Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°..
Melt Temperature 370 - 390 °C
698 - 734 °F
LATI LARPEEK 10 K/40 40% Carbon Fiber Reinforced Polyetheretherketone (PEEK)  (Unverified Data**)
Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°..
Melt Temperature 370 - 390 °C
698 - 734 °F
LATI LARPEEK 50 G/30 30% Glass Reinforced Polyetheretherketone (PEEK)  (Unverified Data**)
Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°..
Melt Temperature 370 - 395 °C
698 - 743 °F
Solvay Specialty Polymers AvaSpire® AV-750 GF40 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-750 GF40 is a 40% glass reinforced polyaryletherketone (PAEK) designed to fill the marketplace need for a lower-priced PEEK (polyetheretherketone). This resin provides the typical chemic..
Melt Temperature 370 - 416 °C
698 - 780 °F
Average value: 392 °C Grade Count:5
Overview of materials for Thermoplastic Polyimide, Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyimide, Carbon Fiber". Each property range of values reported is minimum and maximum va..
Melt Temperature 370 - 400 °C
698 - 752 °F
LATI Larpeek 10 G/50 PEEK, 50% Glass Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Melt Temperature 370 - 400 °C
698 - 752 °F
LATI Larpeek 10 K/30 PEEK, 30% Carbon Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Melt Temperature 370 - 400 °C
698 - 752 °F
LATI Larpeek 10 K/40 PEEK, 40% Carbon Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Melt Temperature 370 - 400 °C
698 - 752 °F
LATI Larpeek 50 G/30 PEEK, 30% Glass Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Melt Temperature 370 - 400 °C
698 - 752 °F
LATI Larpeek 50 K/30 PEEK, 30% Carbon Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Melt Temperature 370 - 400 °C
698 - 752 °F
LATI Larpeek 10 G/15 PEEK, 15% Glass Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Melt Temperature 370 - 400 °C
698 - 752 °F
LATI Larpeek 10 G/30 PEEK, 30% Glass Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Melt Temperature 370 - 400 °C
698 - 752 °F
LATI Larpeek 10 G/40 PEEK, 40% Glass Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Melt Temperature 370 - 400 °C
698 - 752 °F
LATI Larpeek 10 G/60 PEEK, 60% Glass Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Melt Temperature 370 - 400 °C
698 - 752 °F
LATI Larpeek 10 K/20 PEEK, 20% Carbon Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Melt Temperature 370 - 400 °C
698 - 752 °F
LATI Larpeek 10 K/40 HM PEEK, 40% Carbon Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Carbon fiber. High tensile modulus. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Af..
Melt Temperature 370 - 395 °C
698 - 743 °F
Solvay Specialty Polymers AvaSpire® AV-750 GF40 Polyaryletherketone (PAEK), 40% Glass Fiber
AvaSpire® AV-750 GF40 is a 40% glass reinforced polyaryletherketone (PAEK) designed to fill the marketplace need for a lower-priced PEEK (polyetheretherketone). This resin provides the typical ch..
Melt Temperature 370 °C
698 °F
Optimal
BASF Ultrason® E 2010 C6 30% Carbon Filled
Carbon fibers and Ultrason® two partners with good properties. The combination of carbon fibers with the amorphous high-temperature plastic Ultrason® guarantees mechanical properties for temperatu..
Melt Temperature 370 °C
698 °F
Optimal
BASF Ultrason® E 2010 G4 MR SW 15102 20% Glass Filled PESU
Information provided by BASF
Melt Temperature 370 °C
698 °F
Optimal
BASF Ultrason® E 3010 MR UN PESU
Description: Unreinforced, higher viscosity injection molding and extrusion grade with improved toughness and chemical resistance (stress crack resistance); demolding optimized. Abbreviated designat..
Melt Temperature 370 °C
698 °F
Optimal
BASF Ultrason® P 3010 MR SW 10101 PPSU
Description: Unreinforced, higher viscosity injection molding grade, flame retardant and with improved chemical resistance. This grade is black colored and demolding optimized. Abbreviated designati..
Melt Temperature 370 °C
698 °F
Optimal
BASF Ultrason® KR 4113 PESU with 10/10% Carbon Fibers/Graphite and 10% PTFE
Description: Compound based on PES with 30 % filler. The filler system, a mixture of carbon fibers, graphite and PTFE powder, considerably improves Ultrason’s tribological properties. In addition, ..
Melt Temperature 370 - 390 °C
698 - 734 °F
LATI LARPEEK 50 G/20 20% Glass Reinforced Polyetheretherketone (PEEK)  (discontinued **)
Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°..
Melt Temperature 370 - 400 °C
698 - 752 °F
LATI Latilub 88/10-15T G/30 PEEK, 30% Glass Fiber Reinforced, PTFE Filled
Self-lubricating product based on Polyetheretherketone (PEEK). PTFE. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I..
Melt Temperature 370 - 400 °C
698 - 752 °F
LATI Latilub 88/10-15T K/30 PEEK, 30% Carbon Fiber Reinforced, PTFE Filled
Self-lubricating product based on Polyetheretherketone (PEEK). PTFE. Carbon fiber.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I..
Melt Temperature 370 - 400 °C
698 - 752 °F
LATI Latilub 88/50-20GRT K/10 PEEK, 10% Carbon Fiber Reinforced, Graphite/PTFE Filled
Self-lubricating product based on Polyetheretherketone (PEEK). Graphite / PTFE. Carbon fiber. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provid..