Processing Properties Metric English Comments
Melt Temperature 349 - 371 °C
660 - 700 °F
Oxford Polymers PEI 30GF-Natural PEI, 30% Glass Fiber Reinforced
Product Description: Glass Fiber (30% Reinforced), Polyetherimide injection molding grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Release Agents Special Characteristic..
Melt Temperature 20.0 - 371 °C
68.0 - 700 °F
Average value: 184 °C Grade Count:16
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% ar..
Melt Temperature 343 - 371 °C
650 - 700 °F
Molding
PolyOne Lubri-Tech™ PI-10CF/15T Polyetherimide (PEI), Carbon Fiber Reinforced, PTFE Lubricated  (discontinued
Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Melt Temperature 338 - 371 °C
640 - 700 °F
Stock
PolyOne Stat-Tech™ PI-10SS/000 Polyetherimide - 10% Stainless Steel Fiber  (discontinued **)
Data provided by PolyOne.
Melt Temperature 316 - 371 °C
601 - 700 °F
Solvay Specialty Polymers Udel® P-3500 LCD Polysulfone (PSU)  (Unverified Data**)
Udel P-3500 LCD is a very high molecular weight grade of polysulfone, and therefore offers the greatest toughness and chemical resistance of the available grades. It is well-suited for extrusion. Th..
Melt Temperature 360 - 371 °C
680 - 700 °F
LNP Lubricomp® GFL-4034 EM M Polysulfone, Milled Glass Fiber Reinforcement, PTFE Lubricant  (discontinued **)&
Features: Good Moldability, LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP g..
Melt Temperature 360 - 371 °C
680 - 700 °F
LNP Thermocomp® GF-1006 Polysulfone, Glass Fiber Reinforcement  (discontinued **)
Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names..
Melt Temperature 316 - 371 °C
600 - 700 °F
Molding
PolyOne Lubri-Tech™ PI-000/15T Polyetherimide (PEI), PTFE Lubricated  (discontinued **)
Description/Features:PTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Melt Temperature 343 - 371 °C
650 - 700 °F
Molding
PolyOne Edgetek® PI-20GM/000 L Polyetherimide (PEI), Glass Filled  (discontinued **)
Description/Features:Milled Glass Fiber ReinforcedHigh FlowPolyOne First ChoiceInformation provided by PolyOne Corporation.
Melt Temperature 343 - 371 °C
649 - 700 °F
Stock
PolyOne Edgetek® CTXC-084 Polyethersulfone - Mineral Reinforced  (discontinued **)
Data provided by PolyOne.
Melt Temperature 354 - 371 °C
669 - 700 °F
LNP Thermocomp® JF-1006 E LE BK8-055 Polyethersulfone, Glass Fiber Reinforcement  (discontinued **)
Features: High Viscosity, Low ExtractablesForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many L..
Melt Temperature 354 - 371 °C
669 - 700 °F
LNP Thermocomp® JF-1006 EM Polyethersulfone, Glass Fiber Reinforcement  (discontinued **)
Features: Good MoldabilityForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are st..
Melt Temperature 354 - 371 °C
669 - 700 °F
LNP Thermocomp® JF-1008 Polyethersulfone, Glass Fiber Reinforcement  (discontinued **)
Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names..