Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 160 - 170 °C | 320 - 338 °F | |
PolyOne Geon™ Vinyl Wire & Cable JC435XC Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 160 - 170 °C | 320 - 338 °F | |
PolyOne Geon™ Vinyl Wire & Cable JD455CJ Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 160 - 170 °C | 320 - 338 °F | |
PolyOne Geon™ Vinyl Wire & Cable JG513G2 Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 160 - 170 °C | 320 - 338 °F | |
PolyOne Geon™ Vinyl Wire & Cable JG513GO Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 160 - 170 °C | 320 - 338 °F | |
PolyOne Geon™ Vinyl Wire & Cable MA301FA Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 160 - 170 °C | 320 - 338 °F | |
PolyOne Geon™ Vinyl Wire & Cable WJKC505L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Melt Temperature | 160 - 170 °C | 320 - 338 °F | |
PolyOne Geon™ Vinyl Wire & Cable WR7426L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Melt Temperature | 160 - 170 °C | 320 - 338 °F | |
PolyOne Geon™ Vinyl Wire & Cable WY66AL Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 160 - 170 °C | 320 - 338 °F | |
PolyOne Geon™ Vinyl Wire & Cable Y66A Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 160 - 170 °C | 320 - 338 °F | |
PolyOne Geon™ Vinyl Flexible R7426A Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 160 - 170 °C | 320 - 338 °F | |
PolyOne Geon™ Vinyl Wire & Cable MLA71A Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 160 - 170 °C | 320 - 338 °F | |
PolyOne Geon™ Vinyl Wire & Cable WJCK502L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Melt Temperature | 160 - 170 °C | 320 - 338 °F | |
PolyOne Geon™ Vinyl Wire & Cable WY66L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 160 - 170 °C | 320 - 338 °F | |
PolyOne Geon™ Vinyl Flexible R3790B Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 145 - 170 °C | 293 - 338 °F | |
Huntsman IROGRAN® A 70 H 4673 M Polyester-Based TPU-Injection Molding Grade Introduction: IROGRAN A 70 H 4673 M is a soft polyester based thermoplastic polyurethane intended for injection molding applications. IROGRAN A 70 H 4673 M is part of the HUNTSMAN injection molding .. |
|||
Melt Temperature | 165 - 170 °C | 329 - 338 °F | |
Metabolix Mirelâ„¢ P4001 Sheet Extrusion Grade Bioplastic Mirelâ„¢ P4001 is a general purpose, high melt strength material suitable for cast sheet extrusion. Mirelâ„¢ P4001 is designed for a wide range of sheet applications including gift cards, prom.. |
|||
Melt Temperature | 160 - 170 °C | 320 - 338 °F | |
PolyOne Geon™ Vinyl Wire & Cable JG552NP Polyvinyl Chloride Alloy (PVC Alloy) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |