Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 305 - 325 °C | 581 - 617 °F | |
Covestro Apec® DP9-9331 High-Heat Polycarbonate, General Purpose
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Melt Temperature | 305 - 325 °C | 581 - 617 °F | |
Covestro Apec® DP9-9333 High-Heat Polycarbonate, General Purpose, UV-Stabilized
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Melt Temperature | 305 - 335 °C | 581 - 635 °F | |
Covestro Makrolon® CD 2005 Polycarbonate, Optical/Compact Disc Grade
(discontinued **) Injection molding grade with exceptionally good flow, for optical storage media such as CD.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and.. |
|||
Melt Temperature | 305 - 320 °C | 581 - 608 °F | |
Toyobo GLAMIDE® TY-502NZ 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Melt Temperature | 305 - 315 °C | 581 - 599 °F | |
Eurostar Starflam UF0033 PPA, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam UF0033 is a Mineral Flame Retardant, Halogen Free and Red Phosphorous Free, Glass Reinforced, Polyphthalamide Injection Molding ResinInformation provided by Eurostar. |