Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 290 - 320 °C | 554 - 608 °F | |
PolyOne OnForce™ LFT AM-60LGF/001 Natural Polyphthalamide (PPA) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Melt Temperature | 290 - 320 °C | 554 - 608 °F | |
PolyOne OnForce™ LFT NN-40LGF/000 HS UV Black Polyamide 66 (Nylon 66) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Melt Temperature | 290 - 320 °C | 554 - 608 °F | |
PolyOne OnForce™ LFT NN-60LGF/000 HS Natural Polyamide 66 (Nylon 66) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Melt Temperature | 300 - 320 °C | 572 - 608 °F | Injection Molding |
LG Chemical LUPOY GN1006FM PC, Halogen Free, Flame Retardant, Transparency Description: Injection Molding, PC, Halogen Free Flame Retardant, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical |
|||
Melt Temperature | 300 - 320 °C | 572 - 608 °F | Injection Molding |
LG Chemical LUPOY GP1000SW PC, Transparent Description: Injection Molding, PC, General Purpose, TransparencyApplication: Keypad for Mobile Phone, Automotive (Interior)CAS: 103598-77-2Information provided by LG Chemical |
|||
Melt Temperature | 300 - 320 °C | 572 - 608 °F | Injection Molding |
LG Chemical LUPOY GP1006FM PC, Flame Retardant Description: Injection Molding, PC, Flame RetardantApplication: IT/OA, E&E Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical |
|||
Melt Temperature | 280 - 320 °C | 536 - 608 °F | |
LATI Latigloss 66 H2 G/50 F2 PA 66, 50% Glass Fiber Reinforced, Heat Stabilized Product with high mechanical properties and exceptional surface finish based on Polyamide 66 (PA66). Heat stabilized. Glass fibers. Potentially suitable for food/medical contact application. Availab.. |
|||
Melt Temperature | 280 - 320 °C | 536 - 608 °F | |
LATI Latigloss 66 H2 G/60 PA 66, 60% Glass Fiber Reinforced, Heat Stabilized Product with high mechanical properties and exceptional surface finish based on Polyamide 66 (PA66). Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin Am.. |
|||
Melt Temperature | 280 - 320 °C | 536 - 608 °F | |
Covestro Makrolon® 2806 Polycarbonate ISO 7391-PC,M,(,,)-09-9MVR (300 °C/1.2 kg) 9.5 cm3/10 minFood contact qualityMedium viscosityGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CAvailable in transparenttran.. |
|||
Melt Temperature | 280 - 320 °C | 536 - 608 °F | |
Covestro Makrolon® 2867 Polycarbonate, Flame Retardant Grade ISO 7391-PC,MFLR,(,,)-09-9MVR (300 °C/1.2 kg) 9.5 cm3/10 minChlorine- and bromine-free flame retardantUL 94V-2/1.5 mm and 3.0 mmMedium viscosityUV stabilizedEasy releaseInjection molding - Melt tem.. |
|||
Melt Temperature | 280 - 320 °C | 536 - 608 °F | |
Covestro Makrolon® 3156 Polycarbonate ISO 7391-PC,MR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minFood contact qualityHigh viscosityEasy releaseGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CExtru.. |
|||
Melt Temperature | 280 - 320 °C | 536 - 608 °F | |
Covestro Makrolon® 6717 Polycarbonate, Flame Retardant Grade ISO 7391-PC,MFLR,(,,)-05-9Global gradeFormerly Makrolon DP1-1853MVR (300 °C/1.2 kg) 3.0 cm3/10 minFlame retardantUL 94V-0/2.0 mmHigh viscosityBranchedUV stabilizedEasy releaseInjection molding - Me.. |
|||
Melt Temperature | 280 - 320 °C | 536 - 608 °F | |
Covestro Makrolon® LTG3123 Polycarbonate PreprocessingMax. Water content |
|||
Melt Temperature | 280 - 320 °C | 536 - 608 °F | |
Covestro Makrolon® Rx1805 Polycarbonate ISO 7391-PC,M,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minMedical devicesLipid resistantsuitable for sterilization with high-energy radiationComplies with the requirements of FDA-modifie.. |
|||
Melt Temperature | 280 - 320 °C | 536 - 608 °F | |
Covestro Makrolon® T7855 Polycarbonate, Impact Grade ISO 7391-PC,MPR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 12 cm3/10 minImpact modifiedMedium viscosityEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in opaque colors onlyPre.. |
|||
Melt Temperature | 280 - 320 °C | 536 - 608 °F | |
Covestro Makrolon® DP1-1825* Polycarbonate, Impact Grade Developmental productISO 7391-PC,MP,(,,)-09-9MVR (300 °C/1.2 kg) 6.0 cm3/10 minImpact modifiedHigh viscosityInjection molding - Melt temperature 280 - 320 °CAvailable in opaque colors onlyPreproce.. |
|||
Melt Temperature | 280 - 320 °C | 536 - 608 °F | |
Covestro Makrolon® OD2015 Polycarbonate Global gradeOptical storage mediaLow viscosityEasy releaseHigh purityInjection moldingAvailable in natural color onlyPreprocessingMax. Water content |
|||
Melt Temperature | 280 - 320 °C | 536 - 608 °F | |
Akro-Plastic Akromid® A3 GF 25 (2420) PA 6.6 Dry, 25% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Melt Temperature | 280 - 320 °C | 536 - 608 °F | |
Akro-Plastic Akromid® A3 GF 10 (2852) PA 6.6 Dry, 10% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Melt Temperature | 280 - 320 °C | 536 - 608 °F | |
Akro-Plastic Akromid® A3 GF 20 (2419) PA 6.6 Dry, 20% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Melt Temperature | 280 - 320 °C | 536 - 608 °F | |
Akro-Plastic Akromid® A3 GF 40 (1258) PA 6.6 Dry, 40% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Melt Temperature | 280 - 320 °C | 536 - 608 °F | |
Covestro Makrolon® KU1-1230* Polycarbonate ISO 7391-PC,EFL,(,,)-09-9Developmental productMVR (300 °C/1.2 kg) 8.5 cm3/10 minFlame retardant16 mm Triple wall sheet/B1 classification (DIN 4102)Medium viscosityUV stabilizedExtrusionAs of 1 Sept.. |
|||
Melt Temperature | 280 - 320 °C | 536 - 608 °F | |
Covestro Makrolon® LQ2687 Polycarbonate ISO 7391-PC,MLR,(,,)-18-9MVR (300 °C/1.2 kg) 12.5 cm3/10 minOptical lensMedium viscosityUV stabilizedUV 400 cut offEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in clear t.. |
|||
Melt Temperature | 280 - 320 °C | 536 - 608 °F | |
LG Chemical LUCON CP-4208F Conductive Thermoplastic, Flame Retardant LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solvin.. |