Processing Properties Metric English Comments
Melt Temperature 232 - 257 °C
450 - 495 °F
LTL Color Compounds Surlyn Reflection Series® SURSG201UG Surlyn Resin/Nylon 6 Alloy
A patented alloy of DuPont™ Surlyn® resin and nylon 6 for applications that require a high gloss, molded in color surface finish directly from the mold.All information provided by LTL Color ..
Melt Temperature 247 - 257 °C
477 - 495 °F
Solvay Specialty Polymers Ixef® 2060 Polyarylamide (PARA)  (discontinued **)
Ixef 2060 is a 55% reinforced, general purpose polyarylamide compound. This compound exhibits improved vibration resistance, low warpage, and excellent surface finish. This grade has excellent prope..