Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 135 - 305 °C | 275 - 581 °F | Average value: 211 °C Grade Count:16 |
Overview of materials for Ethylene Acrylic Acid This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Acrylic Acid". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Melt Temperature | 135 - 332 °C | 275 - 630 °F | Average value: 298 °C Grade Count:91 |
Overview of materials for Polycarbonate, Carbon Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximum v.. |
|||
Melt Temperature | 135 - 338 °C | 275 - 640 °F | Average value: 286 °C Grade Count:36 |
Overview of materials for Polycarbonate, Stainless Steel Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Stainless Steel Fiber". Each property range of values reported is minimum and maximum val.. |
|||
Melt Temperature | 135 - 152 °C | 275 - 305 °F | |
Clariant PCSP0014 GREY Polycarbonate, Stainless Steel Fiber, EMI Data provided by Clariant Masterbatches |
|||
Melt Temperature | 135 - 152 °C | 275 - 305 °F | |
Clariant Renol PCSP0015 Polycarbonate, Carbon Fiber Filled Data provided by Clariant Masterbatches |
|||
Melt Temperature | 135 - 145 °C | 275 - 293 °F | |
EMS-Griltech Grilon® KA 140 White CoPA Fiber Description: GRILON KA 140 is the standard homo component fusible adhesive fiber. CoPA fiber is characterized by a wide processing window and high adhesive strength.Data provided by EMS-Griltech. |
|||
Melt Temperature | 135 - 145 °C | 275 - 293 °F | |
EMS-Griltech Grilon® KA 140 White CoPA Fiber Description: GRILON KA 140 is the standard homo component fusible adhesive fiber. CoPA fiber is characterized by a wide processing window and high adhesive strength.Data provided by EMS-Griltech. |
|||
Melt Temperature | 135 - 150 °C | 275 - 302 °F | Blow Film Extrusion |
Braskem CN8092 EVA Molding Copolymer CN8092 is an Ethylene-Vinyl Acetate copolymer (EVA) which has a molecular structure that provides easy processing, adhesion, resilience, low hardness, good moisture, and gas barrier properties. It i.. |