Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 720 - 1440 min @Temperature 40.0 °C |
720 - 1440 min @Temperature 104 °F |
|
Abatron AboCast/AboCure 8109-7 Processing: 100/80 pbw; Potlife: 6-7 days/20°C (68°F), 12-24 h/40°C (105°F), 0.75-7 h /60°C (140°F); mix at 50-80°C (120-175°F); cures in: 1 h/100°C (212°F) + 4 h/150°C (300°F) postcure... |