Polymer Property : Pot Life = 1440 min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Pot Life 720 - 1440 min

@Temperature 40.0 °C
720 - 1440 min

@Temperature 104 °F
Abatron AboCast/AboCure 8109-7
Processing: 100/80 pbw; Potlife: 6-7 days/20°C (68°F), 12-24 h/40°C (105°F), 0.75-7 h /60°C (140°F); mix at 50-80°C (120-175°F); cures in: 1 h/100°C (212°F) + 4 h/150°C (300°F) postcure...