Polymer Property : Gel Time = 3.50 min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Gel Time 3.50 - 5.80 min

@Temperature 150 °C
3.50 - 5.80 min

@Temperature 302 °F
Lord Adhesives Thermosetâ„¢ ME-430 Epoxy Board Level Encapsulant
LORD Thermosetâ„¢ ME-430 encapsulant is a onecomponent, semiconductor grade epoxy designed for the encapsulation of Chip-on-Board (COB) devices. It is composed of 100% solids and formulated with ..