Processing Properties Metric English Comments
Annealing Temperature 650 - 825 °C
1200 - 1520 °F
California Fine Wire Copper, 27% Nickel Clad
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.