Processing Properties | Metric | English | Comments |
---|---|---|---|
Annealing Temperature | 650 - 825 °C | 1200 - 1520 °F | |
California Fine Wire Copper, 27% Nickel Clad All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |