Processing Properties | Metric | English | Comments |
---|---|---|---|
Annealing Temperature | 1040 - 1070 °C | 1900 - 1960 °F | Stress Relief Annealing (min. 0.5 h) |
Outokumpu 4841 High Temperature Austenitic Stainless Steel Variant of 1.4845 with an increased silicon content which enhances the steel's resistance to oxidation/corrosion but has also made it more susceptible to embrittlement.Applications: Heat and creep r.. |
|||
Annealing Temperature | 1040 - 1070 °C | 1900 - 1960 °F | Stress Relief Annealing (min. 0.5 h) |
Outokumpu 4845 High Temperature Austenitic Stainless Steel Standardized high-temperature steel for use at temperatures up to 1100°C in dry air. Prone to embrittlement after exposure between 600-900°C. Applications: Heat and creep resistance. For use o.. |
|||
Annealing Temperature | 1040 - 1120 °C | 1900 - 2050 °F | Quench Annealing |
Outokumpu SAF 2507® Duplex Stainless Steel Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone.. |
|||
Annealing Temperature | 1040 - 1120 °C | 1900 - 2050 °F | Stress Relief Annealing |
Outokumpu SAF 2507® Duplex Stainless Steel Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone.. |
|||
Annealing Temperature | 1040 °C | 1900 °F | |
Schmolz + Bickenbach UGIMA® 630 Stainless Steel Bar Description: 630 UGIMA® is an improved machining martensitic precipitation hardenable grade produced only by Ugitech. It is identical in every way to standard type 630 (17-4), except with respect.. |