Processing Properties | Metric | English | Comments |
---|---|---|---|
Shelf Life | 7.00 Month | 7.00 Month | |
Dow Corning 738 ELECTRICAL SEALANT. WHITE Durable general purpose sealant/adhesive for a wide variety of bonding and sealing applications. Can be used in applications where mil spec is required.Information provided by Dow Corning |
|||
Shelf Life | 7.00 Month | 7.00 Month | |
Dow Corning SE 4400 KIT Two-part, grey, heat cure, flowable, thermally conductive, UL V-0.Information provided by Dow Corning |
|||
Shelf Life | 7.00 Month | 7.00 Month | |
Dow Corning SE 9184 WHITE RTV One-part, white, moisture cure RTV, non-flowing, fast tack free, controlled volatility, thermally conductive, UL V-0.Information provided by Dow Corning |
|||
Shelf Life | 7.00 Month | 7.00 Month | |
3M Scotch-Weld™ 1870 Industrial Adhesive Features: A fast drying, highly flexible adhesive with very long tack range and good water resistanceFor bonding fabrics and most other lightweight materials with little or no tendency to stain or b.. |