Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 4.98 - 10.0 min | 0.0830 - 0.167 hour | handling time |
Permabond TA4202 Toughened Acrylic Adhesive PERMABOND® TA4202 is a 2-part, 1:1 toughened acrylic adhesive. It can be used to bond a wide variety of materials including metals, plastics, GRP, ceramics, wood and other substrates. It is conveni.. |
|||
Cure Time | 4.98 - 10.0 min | 0.0830 - 0.167 hour | handling time |
Permabond TA4300 Toughened Acrylic Adhesive PERMABOND® TA4300 is a 2-part, 1:1 toughened acrylic adhesive. Its toughening makes it ideal for bonding dissimilar materials where differential thermal expansion and contraction could be an issue... |
|||
Cure Time | 4.98 - 9.60 min @Temperature 149 °C |
0.0830 - 0.160 hour @Temperature 300 °F |
|
Master Bond Supreme 3HTND-2GT Toughened, Fast Curing, One Part Glob Top Adhesive Master Bond Polymer System Supreme 3HTND-2GT is a fast curing, toughened one component high performance epoxy adhesive/sealant which meets the growing need for precise positioning and bonding of mic.. |
|||
Cure Time | 4.98 min @Temperature 32.0 °C |
0.0830 hour @Temperature 89.6 °F |
Initial Set |
Chesterton ARC 5ES Rapid Repair Stick Description: ARC 5ES is specifically formulated for quick reliable repairs. Its “stick” design combines the performance of a two component system with the convenience of a single component. The AR.. |
|||
Cure Time | 4.98 min @Pressure 0.345 MPa, Temperature 121 °C |
0.0830 hour @Pressure 50.0 psi, Temperature 250 °F |
Recommended Cure Cycle |
Arlon 55986C028 0.0295" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave 1: N/ASide 1: Cured Silicone RubberSubstrate: Style 162 FiberglassSide 2: Uncured Silicone RubberInterleave 2: LDPEThis data represents typical values for the pro.. |