Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 4.98 - 9.60 min @Temperature 149 °C |
0.0830 - 0.160 hour @Temperature 300 °F |
|
Master Bond Supreme 3HTND-2GT Toughened, Fast Curing, One Part Glob Top Adhesive Master Bond Polymer System Supreme 3HTND-2GT is a fast curing, toughened one component high performance epoxy adhesive/sealant which meets the growing need for precise positioning and bonding of mic.. |