Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 2.00 - 4.00 min | 0.0333 - 0.0667 hour | |
Permabond TA4246 Toughened Acrylic Adhesive PERMABOND® TA4246 is a 2-part, no-mix, room temperature curing structural adhesive. It is ideal for use on a wide variety of substrate materials and forms a very high strength structural bond with .. |
|||
Cure Time | 3.00 - 4.00 min | 0.0500 - 0.0667 hour | Working time |
ITW Devcon Flex Bondâ„¢ Methacrylate Adhesive Pipe Sealant, Purple Information provided by ITW Devcon |