Lubrizol Estane® MVT 80AF3 Thermoplastic Polyurethane, Moisture Vapor Transmission

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyether Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Estane® MVT 80AF3 Thermoplastic Polyurethane, Moisture Vapor Transmission.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Type: Estane® MVT 80AF3 TPU is a aromatic polyether-based thermoplastic polyurethane (TPU).Features: High moisture vapor transmission, good low temperature properties and elasticity.Uses: Blown and flat die/cast film extrusion.Available in Americas, Europe, Middle East, Africa, India and AsiaInformation Provided by The Lubrizol Corporation
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D792
Water Vapor Transmission 650 g/m²/day

@Temperature 23.0 °C
41.9 g/100 in²/day

@Temperature 73.4 °F
50% RH, Upright Cup, Water; ASTM E96B
6000 g/m²/day

@Temperature 38.0 °C
386 g/100 in²/day

@Temperature 100 °F
98% RH, Upright Cup, Water; MOCON
9500 g/m²/day

@Temperature 38.0 °C
612 g/100 in²/day

@Temperature 100 °F
90% RH, Upright Cup, Desiccant; ASTM E96E
Melt Flow 54 g/10 min

@Load 8.70 kg,
Temperature 190 °C
54 g/10 min

@Load 19.2 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
ASTM D2240
Hardness, Shore D 77 - 83
77 - 83
ASTM D2240
Tensile Strength, Ultimate 27.6 MPa
4000 psi
ASTM D412/D638
Elongation at Break 800 %
800 %
ASTM D412/D638
Tensile Modulus 0.0138 GPa
2.00 ksi
500%; ASTM D412/D638
100% Modulus 0.00410 GPa
0.595 ksi
ASTM D412/D638
300% Modulus 0.00690 GPa
1.00 ksi
ASTM D412/D638
Tear Strength 16.7 kN/m
95.0 pli
Split Tear Resistance; ASTM D470
68.4 kN/m
390 pli
Die C; ASTM D624
Taber Abrasion, mg/1000 Cycles 81

@Load 1.00 kg
81

@Load 2.20 lb
H-18 wheel; ASTM D3389 B
Compression Set 17 %

@Load 0.0000224 kg,
Temperature 23.0 °C
17 %

@Load 0.0000484 lb,
Temperature 73.4 °F
ASTM D395
Tensile Set 10 %
10 %
200% elongation; ASTM D412
Thermal Properties Metric English Comments
Vicat Softening Point 68.0 °C
154 °F
ASTM D1525
Processing Properties Metric English Comments
Zone 1 166 - 177 °C
331 - 351 °F
Extrusion
Zone 2 170 - 182 °C
338 - 360 °F
Extrusion
Zone 3 177 - 188 °C
351 - 370 °F
Extrusion
Zone 4 182 - 193 °C
360 - 379 °F
Extrusion
Adapter Temperature 182 - 193 °C
360 - 379 °F
Extrusion
Die Temperature 177 - 188 °C
351 - 370 °F
Zone 2, Extrusion
182 - 193 °C
360 - 379 °F
Zone 1, Extrusion
Screw Speed 15 - 40 rpm
15 - 40 rpm