Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Back Pressure = 2470 psi Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Back Pressure 3.00 - 17.0 MPa
435 - 2470 psi
Ascend Performance Materials Vydyne® 66B, 66J Nylon 66, Dry as Molded
Vydyne® 66B and 66J are members of a family of unreinforced extrusion grade Nylon 66 resins. They are available in natural color. These resins offer high strength, rigidity, and toughness for a bro..
Back Pressure 3.00 - 17.0 MPa
435 - 2470 psi
Ascend Performance Materials Vydyne® 65A Nylon 66, General Purpose, intermediate viscosity, DAM
Vydyne® 65A is a medium-viscosity, heat-stabilized PA66 resin suitable for injection-molding extrusion and compounding applications. It is available in natural color only. Vydyne 65A resin offers h..
Back Pressure 3.00 - 17.0 MPa
435 - 2470 psi
Ascend Performance Materials Vydyne® 66B Nylon 66, General Purpose, high viscosity, DAM
Vydyne® 66B is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66B resin offers high strength, ..
Back Pressure 3.00 - 17.0 MPa
435 - 2470 psi
Ascend Performance Materials Vydyne® 66B, 66J Nylon 66, Conditioned (2.5% Moisture)
Vydyne® 66B and 66J are members of a family of unreinforced extrusion grade Nylon 66 resins. They are available in natural color. These resins offer high strength, rigidity, and toughness for a bro..
Back Pressure 3.00 - 17.0 MPa
435 - 2470 psi
Ascend Performance Materials Vydyne® 66J Nylon 66, General Purpose, high viscosity, DAM
Vydyne® 66J is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66J resin offers high strength, ..
Back Pressure 3.00 - 17.0 MPa
435 - 2470 psi
Ascend Performance Materials Vydyne® 66R Nylon 66, General Purpose, high viscosity, DAM
Vydyne® 66R is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66R resin offers high strength, ..
Back Pressure 3.00 - 17.0 MPa
435 - 2470 psi
Ascend Performance Materials Vydyne® 67B Nylon 66, General Purpose, very high viscosity, DAM
Vydyne® 67B is a very-high-viscosity PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 67B resin offers high strength, rigidity and..